Please enable JavaScript.
Coggle requires JavaScript to display documents.
Magnetization Process - Coggle Diagram
Magnetization
Process
Low Magnetic value
in production
Mixing
Process
Change
Recipe
Too much material left in the mixer from previous
recipe (low mag / no mag) . Process mixer closed too soon
Recycle from previous mixer, low mag recipe.
Outside Recycle
Lamination process
Hot Magnetization
Residual Material low mag / no mag
in the piping
Low Temperature material before Mag Roll
Material Temp.in piping/mixer/..
Steel belt too cold
IR temp too low
Setting wrong value
IR lamps KO
Glass too dirty
Direct Cooling water
Cold Magnetization
Residual material low mag/no mag
in the piping
Roll too dirty
Material lose contact with roll
Inline Measurement
Warehouse / Transport
Material can start losing magnet force at temperatures higher than 45°c / 113 F.