Structural Clay and Facing Materials, Fired Bond, Durability,…
-
Fired Bond
-
-
- results in a dense, strong body with significant shrinkage
-
- fused phase forms a glassy matrix
3.porosity,water absorption :arrow_down:
Vitrification :arrow_right: gradual formation of a liquid glass that flows into and fills some of the pore volume
During firing :fire:
-
:check:clay dehydrates,eliminate the hydrating water
-
-
Durability
-
poor design practice :arrow_right: allow adequate expansion joints for dimensional movements can cause failure
-
-
-
-
-
-
-
Texture
-
Methods
-
Molding
forming wet, soft clay into a brick-shaped mold box
Extrusion