casting failures (surface roughness (DUE TO: (too high temp of alloy,…
casting failures
surface roughness
-
-
-
casting force too high, investment cracks
-
incomplete casting
-
-
insufficient heating of alloy, investment
-
-
porosity
-
back pressure porosity
(irregular voids, rounded margins, holes extending thru the casting)
-
-
-
-
-
-
-
surface irregularities
-
-
voids
underheating: wax not eliminated, carbonaceous residue combine with alloy
contamination
-
oxidation due to: never use flux, never use reducing zone, heat alloy too hot
-